1
Yarn & Warping
Ring, slub or open-end warp yarn wound onto beams. Core-spun stretch weft booked for the order.
CHECK · yarn count, strength, slub level
Fabric-Supplier rope-dyes, weaves and finishes stretch, rigid, selvedge, raw, eco and coated denim from 8 to 21 oz in its own mill, and sells it wholesale in full rolls to garment factories, brands and importers.

Six denim families from 8 to 21 oz, sold wholesale in full rolls. Pick a tag for weight, construction, typical use and the problem buyers meet most often.

Women’s jeans, skinny and slim fits, jeggings.

Jackets, workwear, structured jeans and bags.

Premium jeans, raw and heritage collections.

High-end jeans that fade with wear.

Eco collections and the European market.

Streetwear, outerwear and fashion jeans.
Start from the garment. Each choice gives the article, weight, stretch level and the tests to write into your PO.
High stretch with tested recovery so the fit holds all day.
92/6/2 dual-core · 3/1 RHT · stretch ≥ 40%
Classic look; comfort stretch for mainstream, rigid for heritage fades.
99/1 or 100% cotton · 3/1 RHT · sanforized
Enough body to hold the shape of collar, yoke and pockets.
100% cotton · 3/1 RHT or broken twill
Light enough to button and tuck, with a denim look.
100% cotton or lyocell blend · plain or 2/1 twill
Drapes and moves; lyocell adds softness and a cool hand.
Cotton / lyocell, optional 1% elastane · 3/1 twill
Abrasion and tear resistance for daily hard use.
100% cotton · 3/1 RHT · coated option
Denim is sold in oz per square yard (1 oz ≈ 34 g/m²). Weight sets drape and durability; stretch sets fit and comfort.
Holds its shape, fades with high contrast. For heritage jeans, jackets and workwear.
Looks like rigid denim but moves with the body. The standard for straight and slim jeans.
High stretch with tested recovery, for skinny and jegging fits. How recovery is tested
Weight, weave, stretch, color and finish are built to your spec. Send the sheet and we reply with a price and a hand-loom sample.
Most denim claims appear after washing, not on the roll. That is where we test.
Indigo shade drifts within and between dye sets. Every roll is graded on a washed shade blanket, so each lay is cut from one shade group.
32 rolls from three dye sets arrive mixed. The cutting room takes the next roll, so the four panels of one jean come from different shades.
Skewed and sanforized denim stays within 3% shrinkage and 5% skew. Loomstate twill can lose up to 10% in length and twist the leg. Drag the handle to compare.
Baggy knees mean the fabric stretched but did not recover. Growth is tested to ASTM D3107 on every lot — limit ≤ 5%.
Stretch under load: 0%. The part that does not come back after 30 minutes is growth.
MYTHA higher stretch % means a better fit.
FACTFit holds only if the fabric comes back. Growth after 30 minutes is tested to ASTM D3107; the limit is ≤ 5%.
MYTHAny elastane weft gives the same result.
FACTBare elastane that is under-set grows and bags at the knee. We use core-spun or dual-core weft.
MYTHRecovery is fixed once the yarn is chosen.
FACTHeat-setting decides it too, so the setting of every lot is logged.
Wash-down depends on how deep the indigo ring sits in the warp yarn. Each dye set is approved on a washed panel before bulk.
| Ring-dyed · our standard | Over-penetrated · the risk | |
|---|---|---|
| Where indigo sits | Outer ring, white core | Indigo reaches the core |
| After stone washing | High-contrast fade | Washes down flat and dull |
| What decides it | Dip count, airing and bath pH fixed per article | Ring deeper or shallower than on your sample |
Every dye set is approved on a washed panel before bulk, so the wash-down matches the sample you sold from.
Wet crocking is the most common failure on dark and black denim. Wash-off after dyeing and fixing agent keep it in the PO grade.
| Test cloth | Not washed-off | Washed-off & fixed |
|---|---|---|
| Dry AATCC 8 | 3 | 4–5 |
| Wet ISO 105-X12 | 1–2 | 3 |
| Why | Surface indigo and sulfur left on the yarn | Wash-off boxes after dyeing; fixing agent on dark & black |
| In the PO | No grade — no basis for a claim | Dry ≥ 3–4 · Wet ≥ 2–3 per lot |
The same fabric looks different after washing. Every dye set gets a panel washed to your recipe, so you approve the finished look.
Wash recipes are run on production machines in our own laundry. Types of denim washing
Six stages under one roof, each with a fixed check before the fabric moves on.

Ring, slub or open-end warp yarn wound onto beams. Core-spun stretch weft booked for the order.

Ropes of warp yarn dipped and aired in indigo, optional sulfur bottom or top.

3/1 right-hand, left-hand or broken twill on wide air-jet or shuttle looms for selvedge.

Singeing, skewing, heat-setting for stretch, then compressive shrinking.

4-point inspection of every roll, shade blanket and wash panel for every set.

Rolls ticketed, wrapped and loaded by shade group under supervision.
Core articles in regular production; send a swatch for anything else. Composition and construction are reference values — replace with your real specs.
| Article | Composition | Weave | Weight | Stretch | Typical Use | MOQ |
|---|---|---|---|---|---|---|
| Comfort Stretch Denim | 98% cotton / 2% elastane | 3/1 RHT | 10.5 oz | 20–25% | Women's jeans | 500 m |
| Power Stretch Denim | 92/6/2 dual-core | 3/1 RHT | 9.5 oz | 40–60% | Skinny jeans | 500 m |
| Rigid Denim | 100% cotton | 3/1 RHT | 13 oz | — | Straight jeans | 500 m |
| Heavyweight Denim | 100% cotton | 3/1 RHT | 16 oz | — | Jackets, workwear | 500 m |
| Selvedge Denim | 100% cotton | 3/1 RHT · shuttle | 14 oz | — | Premium jeans | 500 m |
| Raw Denim | 100% cotton | 3/1 LHT | 12.5 oz | — | Heritage jeans | 500 m |
| Lyocell-Blend Denim | 70% cotton / 30% lyocell | 3/1 RHT | 9 oz | 0–15% | Dresses, shirts | 500 m |
| Chambray Shirting | 100% cotton | Plain | 5.5 oz | — | Shirts | 500 m |

Tested to AATCC, ASTM and ISO methods and reported with every shipment. Stricter limits can go into your PO.
OEKO-TEX Standard 100 and ISO 9001:2015, listed with numbers so you can verify them directly.
Six garment lines our buyers make, with the weight we usually supply for each.






Six reasons, each linked to a control on this page.
Rope dyeing, weaving and sanforizing under one quality system.
Rolls graded after washing, not just raw.
Core-spun weft and ASTM D3107 growth tests.
8–21 oz, RHT / LHT / broken twill, developed from your sample.
Roll tickets, packing lists and test reports ready for customs and buyers.
Existing swatches free of charge; you only cover the courier.
Six steps from inquiry to shipment; bulk ships 20–35 days after the wash panel is approved.
Garment, weight, stretch, quantity and a photo or swatch.
Existing articles free; courier paid by buyer.
For custom articles, a hand-loom sample and a panel washed to your recipe.
Dye set and stretch yarn reserved, ship date confirmed in writing.
Weekly photos and status on WhatsApp.
4-point report, shade blanket, test reports and roll tickets.
Quoted per meter on EXW, FOB, CIF or DDP. Six choices move the price most — send your spec for an exact quote.
| Factor | Lower price | Higher price |
|---|---|---|
| Weight | 8 oz | 14.5–18 oz+ |
| Stretch | Rigid | Power stretch / dual-core |
| Dyeing | Indigo or sulfur black | Indigo + sulfur |
| Loom | Wide loom | Selvedge (shuttle loom) |
| Fiber | Cotton | Organic, recycled or lyocell blend |
| Quantity | 50,000 m+ | 500 m |
Send garment, weight, stretch, fiber and quantity — we reply with a price per meter within one working day.
Index values are illustrative — replace with your real price ratios.
Buyers who come to us for denim fabric supplier often source several fabrics in one program. These pages use the same order terms — 500 m MOQ, 20–35 days — and can share one container.
Can’t find your answer? Message us on WhatsApp — we usually reply within one working day.
500 meters per order. Swatches of existing articles are free; you only pay the shipping.
Denim fabric price is quoted per meter and depends mainly on weight, stretch, dyeing, loom type, fiber and quantity — see what determines denim fabric price.
Yes. All articles ship as denim fabric rolls of about 100 yards, each with a roll ticket showing weight, cuttable width, shade group and shrinkage.
Yes. Selvedge denim fabric from 12 to 16 oz and raw denim fabric from 10 to 15 oz. See What Is Selvedge Denim.
Usually 20–35 days for bulk after the wash panel is approved.
We are a denim fabric manufacturer with our own dyeing, weaving and finishing, so bulk denim fabric orders are produced and tested under one quality system.
Yes. We analyze weave, yarn and indigo depth, then send a hand-loom sample and a washed panel for approval.
T/T bank transfer, PayPal and XTransfer. Deposit and balance are agreed per order.
Shrinkage, skew, stretch and growth, crocking, washing fastness, tear strength, weight and cuttable width.
Garment, weight, stretch and quantity are enough to start.